Pump & Valve Material Selection Guide: Matching Media to Materials

For: Design engineers or consultants selecting pump and valve materials for water treatment, chemical, petrochemical, desalination and other projects.

Why Material Selection Matters

Consequences of Wrong Material:

  • Corrosion perforation: Seawater pump in plain carbon steel rusts through in months; sulfuric acid pipe in 304 stainless pits and leaks within a year.
  • Performance degradation: Corroded impeller becomes thinner, pump flow and head drop; corroded valve core loses seal, leakage increases.
  • Safety incidents: High-temperature high-pressure pipe corrodes and ruptures, medium sprays out, causing casualties or environmental pollution.

Article objective: Provide a quick reference table and decision flow for selecting pump and valve materials based on medium and operating conditions.

I. Classification of Common Pump & Valve Materials

1. Cast Iron

Grades: HT200, HT250 (gray iron), QT450 (ductile iron)

Characteristics:

  • Low cost, good castability, suitable for mass production.
  • Average wear resistance, poor impact resistance (gray iron brittle).
  • Not acid/alkali resistant, rusts even in slightly corrosive environments.

Applications:

  • Fresh water, cooling water, low-temperature (< 80°C) non-corrosive media.
  • Low-pressure systems (PN ≤ 16).

Not suitable: Seawater, acids/alkalis, high temperature (> 200°C), high pressure.

2. Carbon Steel

Grades: WCB (ASTM A216), 20#, Q235 (GB)

Characteristics:

  • High strength, pressure-resistant, high-temperature tolerant (< 450°C).
  • Not corrosion-resistant, requires coating or lining protection.

Applications:

  • Fresh water, steam, oils, non-corrosive chemical liquids.
  • Medium-high pressure systems (PN 16–100).

Not suitable: Seawater, acids/alkalis, chloride environments.

3. Stainless Steel

3.1 Austenitic Stainless Steel

304 (CF8, 1.4301):

  • Composition: 18% Cr + 8% Ni
  • Features: General-purpose stainless, resists general corrosion, good machinability.
  • Suitable: Fresh water, food, pharmaceuticals, general chemicals.
  • Not suitable: Seawater (pitting), strong acids/alkalis, high-chloride environments.

316 (CF8M, 1.4401):

  • Composition: 18% Cr + 10% Ni + 2% Mo (molybdenum)
  • Features: Better corrosion resistance than 304, especially chloride pitting resistance.
  • Suitable: Seawater (short-term), brine, weak acids/alkalis, pharmaceuticals.

316L (ultra-low carbon):

  • Features: Carbon < 0.03%, better weldability, resists intergranular corrosion.
  • Suitable: Seawater, brine, food (sanitary grade), pharmaceuticals, nuclear power.

2205 (Duplex Stainless, S31803):

  • Composition: 22% Cr + 5% Ni + 3% Mo
  • Features: High strength (2× 316), resists pitting, crevice corrosion, stress corrosion.
  • Suitable: Seawater, brine, chloride environments, offshore platforms, desalination.
  • Cost: 50–80% more than 316L, but longer life, possibly lower total cost.

4. Nickel Alloys

Hastelloy C-276:

  • Composition: 57% Ni + 16% Cr + 16% Mo + 5% W
  • Features: Resists strong acids/alkalis, high-temperature oxidation, reducing environments.
  • Suitable: Concentrated sulfuric acid, hydrochloric acid, chlorine, wet chlorine, phosphoric acid.
  • Cost: Very expensive (10–20× 316L), only for extreme corrosion environments.

Monel 400:

  • Composition: 67% Ni + 30% Cu
  • Features: Resists seawater, hydrofluoric acid, alkaline solutions.
  • Suitable: Seawater systems, offshore drilling platforms, hydrofluoric acid transport.

5. Titanium Alloys

TA2 (Commercial Pure Titanium, Gr.2):

  • Features: Resists seawater, brine, chlorides, nitric acid, lightweight (60% density of steel).
  • Suitable: Desalination, offshore platforms, chlor-alkali industry.
  • Drawbacks: Expensive (5–10× 316L), difficult to machine.

6. Linings & Coatings

Rubber Lining:

  • Natural Rubber (NR): Wear-resistant, suitable for slurry transport (mining, slurry pumps).
  • Neoprene (CR): Resists seawater, brine, dilute acids/alkalis.

PTFE Lining (Fluoropolymer):

  • Features: Resists almost all chemicals (except molten alkali metals and fluorine), temp range -200°C to +200°C.
  • Suitable: Strong acids/alkalis, organic solvents, high-purity media.
  • Drawbacks: High cost, low mechanical strength, prone to wear.

Glass-Lined:

  • Features: Excellent acid resistance (except HF and hot concentrated phosphoric acid), smooth non-stick surface.
  • Suitable: Pharmaceutical, food, fine chemical reactors, tanks, piping.
  • Drawbacks: Brittle, sensitive to impact and thermal shock.

II. Material Selection by Medium

Medium Recommended Material Not Recommended Notes
Fresh Water (Tap) Cast iron, carbon steel, 304 – Temp < 80°C use cast iron; > 80°C use carbon steel
Seawater 316L, 2205, Titanium Cast iron, carbon steel, 304 304 pits; 316L short-term OK, long-term use 2205
Wastewater Cast iron, carbon steel (coated), 316L – With chlorides or pH < 6 use 316L
Brine (High Chloride) 316L, 2205, Titanium 304, plain carbon steel Chloride > 200ppm use 316L or 2205
Sulfuric Acid (< 80%) 316L, Hastelloy C-276 Carbon steel, 304 Conc. < 10% can use 316L; > 10% use Hastelloy
Hydrochloric Acid Hastelloy C-276, PTFE lining All stainless, carbon steel Stainless corrodes rapidly in HCl
Sodium Hydroxide (Caustic) Carbon steel, Monel 400 Aluminum, zinc, tin Conc. < 50%, temp < 80°C use carbon steel
Ammonia Solution Carbon steel, 304, 316L Copper alloys, zinc Copper corroded by ammonia
Diesel, Gasoline Carbon steel, 304 Rubber (swells) High-sulfur diesel use 316
Steam (> 200°C) Carbon steel (WCB), alloy steel Cast iron (brittle), rubber High-pressure steam (> 16bar) use alloy steel
Liquid Chlorine, Chlorine Gas Hastelloy C-276, Titanium, PTFE All stainless steel Wet chlorine highly corrosive, dry chlorine use carbon steel

III. Material Selection by Temperature

Temperature Range Suitable Materials Not Suitable
< -20°C (Low Temp) 304, 316L, aluminum alloys Cast iron (brittle), carbon steel (low-temp embrittlement)
-20°C ~ 200°C Cast iron, carbon steel, 304, 316 –
200°C ~ 450°C Carbon steel (WCB), alloy steel Cast iron, rubber, PTFE
> 450°C (High Temp) Alloy steel (e.g. A217 WC9), 310 stainless Carbon steel (creep), rubber

IV. Material Selection Decision Flow

Step 1: Identify Medium Type

  • Fresh water, steam, oils → Carbon steel or cast iron (with coating).
  • Seawater, brine → 316L or 2205.
  • Strong acids/alkalis → Hastelloy or PTFE lining.

Step 2: Check Chloride Content

  • < 100 ppm: 304 usable.
  • 100–1000 ppm: 316L.
  • > 1000 ppm: 2205 or titanium.

Step 3: Check Temperature

  • < 80°C: Cast iron, 304 usable.
  • 80–200°C: Carbon steel, 316L.
  • > 200°C: Carbon steel or alloy steel.

Step 4: Check Pressure

  • PN ≤ 16: Cast iron usable.
  • PN 16–40: Carbon steel, 304, 316.
  • PN > 40: Carbon steel forgings, alloy steel.

Step 5: Consider Cost vs Life

  • CAPEX priority: Choose cheaper materials (e.g. carbon steel + coating).
  • LCCA priority: Choose corrosion-resistant materials (e.g. 316L, 2205), though expensive, but longer life, less maintenance.

V. Common Material Standard Equivalents

China GB US ASTM Europe EN Common Name
ZG230-450 WCB GS-C25 Carbon Steel
0Cr18Ni9 304 (CF8) 1.4301 Stainless 304
00Cr17Ni14Mo2 316L (CF3M) 1.4404 Stainless 316L
00Cr22Ni5Mo3N 2205 (CD3MN) 1.4462 Duplex Stainless
TA2 Gr.2 3.7035 Commercial Pure Titanium

VI. Special Application Material Selection

1. Seawater Desalination

Recommended: 2205 duplex stainless, titanium alloy (TA2). Reason: Seawater chloride > 19,000 ppm, 316L pits, 2205 or titanium is optimal.

2. Solid Particles (Slurry, Ore Pulp)

Recommended: High-chromium iron (Cr26), rubber lining, ceramic lining. Reason: Abrasion is main issue, stainless has poor wear resistance compared to high-chrome or linings.

3. High-Purity Media (Pharma, Semiconductor)

Recommended: 316L or 2205 electropolished surface. Reason: Surface roughness Ra < 0.4μm, no contamination retention, easy cleaning.

4. Food Sanitary Grade

Recommended: 304 or 316L, complying with FDA, 3A, EHEDG standards. Reason: Non-toxic, odorless, resists cleaning agents (e.g. CIP alkaline solution).

Summary: Right Material = Double Equipment Life

3 Principles:

  1. Medium first: Check medium pH, chlorides, temperature, then select material.
  2. Don’t penny-pinch to pound-foolish: 316L is 30% more than 304, but lasts 10× longer in seawater.
  3. Consult experts: Complex conditions (mixed media, high temp/pressure) require materials engineer or supplier consultation.

If you are sourcing pumps, valves or related equipment for a project, send KFE your equipment list and operating data and we will help with selection and quotation.

Related industry: Chemical & Pharmaceutical

Related Products

Send Us Your Equipment List or Operating Conditions

Tell us what you need. KFE handles the quote, specs and delivery, with one contact for you.

Contact KFE